Stabilized Composite Zirconia
|
Component(ZrO2+HfO2) |
≥94% |
|
Composite stabilizing agent |
3.7-4.5 |
|
Fe2O3 |
≤0.1% |
|
SiO2 |
≤0.4% |
|
Al2O3 |
≤0.35% |
|
Use Temperature |
2200 ℃ |
|
Refractoriness |
2400 ℃ |
|
Stability |
70-80 |
Stabilized zirconia can be used to make crucible for vacuum induction melting, high purity zirconium sizing nozzle or zirconium composite long nozzle brick for steelmaking, furnace lining with ultra-high temperature above 1800 ℃ and lining brick for gas reaction furnace.